以丙烯酰胺辅助柠檬酸为络合试剂,采用溶胶-凝胶燃烧法制备La0.6Sr0.4Co1-xMnxO3催化剂(x=0.3、0.5、0.7)并与La Co O3进行比较,进行XRD、BET、SEM、XPS和苯的催化氧化性能和稳定性表征。结果表明,催化活性顺序为:La0.6Sr0.4Co0.7Mn0.3O3>La0.6Sr0.4Co0.5Mn0.5O3>La0.6Sr0.4Co0.3Mn0.7O3>La Co O3。La0.6Sr0.4Co1-xMnxO3催化剂生成钙钛矿相的同时还伴生少量Sr CO3杂相。与La Co O3对比,La0.6Sr0.4Co1-xMnxO3催化剂拥有更大的比表面积、孔容和抗...