Abstract:
采用共沉淀法、沉积-沉淀法和改性沉积-沉淀法制备了Au/Fe2O3催化剂,运用N2吸附、X射线衍射、X射线光电子能谱和透射电镜等技术对其进行了表征,考察了制备方法对Au/Fe2O3催化剂水煤气变换反应催化活性的影响.结果表明,改性沉积-沉淀法制备的催化剂具有最好的催化活性,150 ℃时CO转化率达82.3%.该催化剂比表面积较大,金粒子尺寸(3~5 nm)较小且分布均匀.载体氧化铁以无定形态和结晶态共存,金与载体间存在较强的相互作用,这对催化剂活性的提高起着重要作用.