Indexed by:
Abstract:
An effective way of integrating purification and modification is used for casting the A356 Al alloy. Self-generated inclusion-eliminating flux exhibits excellent purification in the alloy with an inclusion-removal rate of 74 %. The grains of eutectic silicon are fine or vermicular, and diffusely distributed in the A356 Al alloy at a 0.012 w/% Sr addition. The mechanical properties of the alloy are significantly improved, including a tensile strength of 208.5 MPa and an elongation of 17.5 %. As the Sr addition is increased, the comprehensive properties of the material are not improved. The Sr addition can be reduced to a certain degree during the modification of the melt after high purification. The addition of 0.012 w/% Sr is most preferable in the alloy.
Keyword:
Reprint 's Address:
Email:
Source :
MATERIALI IN TEHNOLOGIJE
ISSN: 1580-2949
Year: 2021
Issue: 3
Volume: 55
Page: 443-448
0 . 6 5
JCR@2021
0 . 6 0 0
JCR@2023
ESI Discipline: MATERIALS SCIENCE;
ESI HC Threshold:142
JCR Journal Grade:4
CAS Journal Grade:4
Cited Count:
SCOPUS Cited Count: 7
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 1
Affiliated Colleges: