Inventor:

陈奇俤 (陈奇俤.) [1] (Scholars:陈奇俤) | 易明杰 (易明杰.) [2] | 蔡道平 (蔡道平.) [3] (Scholars:蔡道平) | 詹红兵 (詹红兵.) [4] (Scholars:詹红兵)

Indexed by:

incoPat

Abstract:

本发明公开了一种硫化镍/碳化三聚氰胺泡沫复合电极材料及其制备方法,首先将三聚氰胺泡沫放置于管式炉中,煅烧碳化,得到碳化的三聚氰胺泡沫备用。将Ni2SO4和K2S2O4分别溶于甲醇中,搅拌均匀后混合,再往混合溶液中滴加氨水。之后将碳化后的三聚氰胺泡沫浸润在溶液中,静置2 h后取出,反复用去离子水冲洗后冷冻干燥。将样品与硫粉放置于管式炉中煅烧,便可得到负载于三聚氰胺泡沫上的NiS2材料,该材料表现出优异的电化学性能,包括良好的比电容,优异的倍率性能和良好的循环性能。

Keyword:

Reprint 's Address:

Email:

Show more details

Related Keywords:

Related Article:

Patent Info :

Type: 发明授权

Patent No.: CN201910631133.1

Filing Date: 2019/7/12

Publication Date: 2020/11/27

Pub. No.: CN110265226B

公开国别: CN

Applicants: 福州大学

Legal Status: 授权

Cited Count:

WoS CC Cited Count: 0

SCOPUS Cited Count:

ESI Highly Cited Papers on the List: 0 Unfold All

WanFang Cited Count:

Chinese Cited Count:

30 Days PV: 6

Online/Total:52/10132084
Address:FZU Library(No.2 Xuyuan Road, Fuzhou, Fujian, PRC Post Code:350116) Contact Us:0591-22865326
Copyright:FZU Library Technical Support:Beijing Aegean Software Co., Ltd. 闽ICP备05005463号-1