三级软锰矿粉与无烟煤按4:1~5:1比例混合焙烧后,用氨基甲酸铵溶液浸取,浸出液在80—81℃下分解,得重质MnCO_3,再经330~350℃煅烧,生成含MnO_280%以上的粗品,用Na_2CO_3重质化后,得含MnO_293%以上的成品,其晶型为r型、蜜度为2.1~2.2g/ml,放电性能良好。