首次利用含铬钙镁渣为原料烧制陶瓷砖,并测试了其晶相组成、吸水率、收缩率和可溶性六价铬含量.实验结果表明,最佳掺渣量为15%,并且当烧制温度为1000-1150℃时,主晶相为钙长石,此时解毒彻底,物理性能达到国家内墙砖的标准.