Abstract:
以马来酸酐(MA)、丙烯酸(AA)和丙烯酰胺(AM)为原料,研制出环保型三元共聚阻垢剂PMAA,并通过研究其阻垢性能确定了产品的最佳工艺配方.实验结果表明,当单体的质量配比m(AA)∶ m(AM)∶ m(MA)=2∶ 3∶ 0.5,引发剂用量为单体总质量的1.5%,反应温度为80 ℃,单体质量分数为15%时,得到的聚合物PMAA的用量为5 mg/L时,用国标法测得其对碳酸钙的阻垢率达94.15%,对磷酸钙的阻垢率达80.93%.