采用水热法制备出纯相的NiFe2O4纳米颗粒。利用X射线衍射仪(XRD),透射电镜(TEM)和傅里叶变换红外光谱仪(FT-IR)对样品进行了表征,并运用热分析法和质谱仪研究了样品对高氯酸铵的热分解催化性能。结果表明,制备的NiFe2O4纳米颗粒粒径约为5.0nm,对高氯酸铵的热分解具有很高的催化活性。当NiFe2O4纳米颗粒的添加量达到10%时,对高氯酸铵的热分解催化性能最好,可使高氯酸铵的高温分解温度降低89.8℃。