某选铁尾矿含钼0.031%,为了有效回收其有价金属,在工艺矿物学的基础上,进行了浮选试验研究.结果表明,试验采用粗精矿再磨的工艺流程,进行了"一粗七精三扫",得到含锌0.75%、锌回收率0.42%,含钼46.11%、钼回收率为67.49%的钼精矿.